Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits water cooling. BOHLER W302 is also available int eh special grades ISODISC and ISOBLOC with improved homogeneity and increased toughness. Application:Heavy duty hot work tools and dies, mainly for light alloy processing: mandrels, dies, and containers for metal tube and rod extrusion, hot extrusion equipment; tools and dies for the manufacture of hollow bodies, screws, rivets, nuts and bolts. Die casting equipment, forming dies, die inserts, hot shear blades, and plastic molding dies. |
AISI H13; DIN 1.2344; JIS SKD61; ISO 40CrMoV5 |