MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® 5143N Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Homopolymer for Clear, Thermoformed Components

Formolene® 5143N is a higher melt flow polypropylene homopolymer designed for faster cycle time and excellent clarity. It contains a unique combination of stabilizers and nucleation that provide an excellent balance of stiffness and impact strength. Formolene® 5143N does not contain animal derived ingredients, and is suitable for high temperature food processing and preparation.

Formolene® 5143N meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact. Additionally, it meets FDA requirements regarding retort food processing.

Specimens were injection molded according to the conditions specified in ASTM D4101

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 3.0 g/10 min
@Temperature 230 °C
3.0 g/10 min
@Temperature 446 °F
I2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 38.6 MPa5600 psi2" (50mm) per min; ASTM D638
Elongation at Yield 7.0 %7.0 %2" (50mm) per min; ASTM D638
Flexural Modulus, 1% Secant 1720 MPa250000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.427 J/cm
@Temperature 23.0 °C
0.800 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCPQ009 / 150241

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.