MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Saint-Gobain COHRlastic® CF4444 Reversion Resistant Reinforced Solid Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six constructions. CF 4444 has a specially formulated rubber compound to give better reversion resistance. The reinforcement is a special crush-resistant fiberglass, making the product excellent for press pads in high-temperature and pressure lamination applications. All data based on a 0.0625 inch test sample.(Also available in 3/32, 1/8; Thickness shown is for silicone rubber. Fiberglass thickness = 0.135".)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content <= 0.50 g/l<= 0.50 g/lWeight Loss (4 hrs at 400°F)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979
Elongation at Break <= 10 %<= 10 %
Flexural Strength 5.52 MPa800 psiDiaphragm Burst Strength
Tear Strength 70.1 kN/m400 pli
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 19.7 kV/mm500 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
150 µin/in-°F
@Temperature 68.0 °F
Silicone rubber component
Thermal Conductivity 0.274 W/m-K1.90 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® G1657 M (SEBS) Linear Block Copolymer
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Translink 555
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 290ºF Cure Temperature
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 60A
Mearthane Durethane™ S DS-660A Solid Polyurethane Elastomer

PSTGQZ249 / 68763

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.