MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® G1657 M (SEBS) Linear Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form identified:
Kraton G1657 MS - supplied as a dusted pellet
Kraton G1657 MO - supplied as a dusted pellet

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1657 M is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; and Personal Care

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D4025
Volatiles <= 1.0 %<= 1.0 %KM 04
Brookfield Viscosity 1200 - 1800 cP
@Temperature 25.0 °C
1200 - 1800 cP
@Temperature 77.0 °F
20% Toluene solution; BAM 922
Melt Flow 22 g/10 min
@Load 5.00 kg,
Temperature 230 °C
22 g/10 min
@Load 11.0 lb,
Temperature 446 °F
Ash 0.020 - 0.12 %0.020 - 0.12 %For G1657 MS, Silica dusted; BAM 908
 
Chemical PropertiesMetricEnglishComments
Diblock Content 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 474710 seconds. Typical values on polymer compression molded at 150°C (300°F).; ASTM D2240
Tensile Strength, Ultimate 23.44 MPa3400 psiTypical properties based on film cast from toluene solution.; ASTM D412
Elongation at Break 750 %750 %Typical properties based on film cast from toluene solution.; ASTM D412
300% Modulus 2.41 MPa
@Strain 300 %
350 psi
@Strain 300 %
film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentDust, O0.45-0.75%, KM 1029
 Non-staining phenolic antioxidant0.03-0.10%, KM 08
 Polystyrene12.3-14.3%, KM 03, Measured on the polymer before hydrogenation
 Total Extractables<1.5%, KM 05
Styrene/Rubber ratio13/87

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® G1650 E (SEBS) Linear Block Copolymer
Kraton® FG1924 G (SEBS) Linear Block Copolymer
Kraton® G1652 E (SEBS) Linear Block Copolymer
Kraton® G1654 E (SEBS) Linear Block Copolymer
Kraton® G1765X (EP)n Multi-Arm Copolymer

PKRA0270 / 49087

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.