MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess MACROLEX® Orange 3G Orange Pigment
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Perinone dyestuff

Main fields of application: Transparent and opaque dyeing of PS, SAN, PMMA, PC, PA 6 and PA 6.6.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.110 g/cc0.00397 lb/in³DIN ISO 787-11
Density 1.43 g/cc0.0517 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 230 °C446 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  22 %
@Thickness 2.00 mm,
Wavelength 460 nm
22 %
@Thickness 0.0787 in,
Wavelength 460 nm
0.01% Dyestuff
 43 %
@Thickness 2.00 mm,
Wavelength 360 nm
43 %
@Thickness 0.0787 in,
Wavelength 360 nm
0.01% Dyestuff
 59 %
@Thickness 2.00 mm,
Wavelength 390 nm
59 %
@Thickness 0.0787 in,
Wavelength 390 nm
0.01% Dyestuff
 60 %
@Thickness 2.00 mm,
Wavelength 450 nm
60 %
@Thickness 0.0787 in,
Wavelength 450 nm
0.003% Dyestuff
 68 %
@Thickness 2.00 mm,
Wavelength 360 nm
68 %
@Thickness 0.0787 in,
Wavelength 360 nm
0.003% Dyestuff
 78 %
@Thickness 2.00 mm,
Wavelength 385 nm
78 %
@Thickness 0.0787 in,
Wavelength 385 nm
0.003% Dyestuff
 90 %
@Thickness 2.00 mm,
Wavelength 580 nm
90 %
@Thickness 0.0787 in,
Wavelength 580 nm
0.003% Dyestuff
 90 %
@Thickness 2.00 mm,
Wavelength 580 nm
90 %
@Thickness 0.0787 in,
Wavelength 580 nm
0.01% Dyestuff
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess MACROLEX® Red E2G Red Pigment
Lanxess MACROLEX® Red B Red Pigment
Lanxess MACROLEX® Orange R Gran Orange Pigment
Lanxess MACROLEX® Green 5B Green Pigment
Lanxess MACROLEX® Blue RR Blue Pigment

PLANY8873 / 209265

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.