MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® LX9008 BK 9.7504 Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9008 BK 9.7504 is a plasticizer-free polyamide 12 compound, with an especially high long-term resistance under thermal load. VESTAMID® LX9008 BK 9.7504 is suitable to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel. The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions. Using VESTAMID® LX9008 BK 9.7504 for fuel lines one must pay attention to certain preconditions. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: High heat resistant
Color: Black
Additives: Heat stabilizer
Chemical Resistance: Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 1.40 %Sim to ISO 62
Moisture Absorption 0.700 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00200 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0190 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73.0
@Time 3.00 sec
ISO 7619-1
Tensile Strength at Break 49.0 MPaISO 527
Tensile Strength 41.0 MPaISO 527
Tensile Stress 38.0 MPa
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 41.0 MPaISO 527
Elongation at Break 150 %nom. strain at br., etB; ISO 527
 165 %Nominal; ISO 527
Elongation at Yield 5.00 %ISO 527
Tensile Modulus 1450 MPaISO 527
Flexural Strength 48.0 MPaISO 178
Flexural Modulus 1190 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 22.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
Type of failure: P; ISO 179/1eA
Impact 0.000
@Temperature -40.0 °C
Cold impact resistance, breaks of 10, 912g; Tube dimension; SAE J2260, J2043
 0.000
@Temperature -40.0 °C
Cold impact resistance, breaks of 10, 454g; SAE J844
 0.000
@Temperature -40.0 °C
Cold impact resistance, breaks of 10, 454g; Pretreatment: 2h boiling water; SAE J844
 0.000
@Temperature -40.0 °C
Cold impact resistance, breaks of 10, 454g; Pretreatment: 24h 110°C; SAE J844
 0.000
@Temperature -40.0 °C
Cold impact resistance, breaks of 10, 880g;
 NB
@Temperature -40.0 °C
with pendulum, pipe; Tube dimension: OD x WT 8x1 mm; DIN 73378
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Dielectric Constant 2.90
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 3.70
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 37.0 kV/mmAC, S20/P50; Sim. To IEC 60243-1
 38.0 kV/mmAC, S20/S20, t.; IEC 60243-1
Dissipation Factor 0.0320
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0520
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.5 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 176 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 113 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CISO 75-1/-2
Vicat Softening Point 145 °C
@Load 5.10 kg
50 K/h; ISO 306
 175 °C
@Load 1.02 kg
50 K/h; ISO 306
Glass Transition Temp, Tg 47.0 °CISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7918 / 325050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.