MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® LX9008 BK 9.7504 Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9008 BK 9.7504 is a plasticizer-free polyamide 12 compound, with an especially high long-term resistance under thermal load. VESTAMID® LX9008 BK 9.7504 is suitable to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel. The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions. Using VESTAMID® LX9008 BK 9.7504 for fuel lines one must pay attention to certain preconditions. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: High heat resistant
Color: Black
Additives: Heat stabilizer
Chemical Resistance: Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption 1.40 %1.40 %Sim to ISO 62
Moisture Absorption 0.700 %0.700 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00200 cm/cm0.00200 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0190 cm/cm0.0190 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73.0
@Time 3.00 sec
73.0
@Time 0.000833 hour
ISO 7619-1
Tensile Strength at Break 49.0 MPa7110 psiISO 527
Tensile Strength 41.0 MPa5950 psiISO 527
Tensile Stress 38.0 MPa
@Strain 50.0 %
5510 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 41.0 MPa5950 psiISO 527
Elongation at Break 150 %150 %nom. strain at br., etB; ISO 527
 165 %165 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 1.45 GPa210 ksiISO 527
Flexural Strength 48.0 MPa6960 psiISO 178
Flexural Modulus 1.19 GPa173 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  2.20 J/cm²
@Temperature -30.0 °C
10.5 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Type of failure: P; ISO 179/1eA
Impact  0.000
@Temperature -40.0 °C
0.000
@Temperature -40.0 °F
Cold impact resistance, breaks of 10, 912g; Tube dimension; SAE J2260, J2043
 0.000
@Temperature -40.0 °C
0.000
@Temperature -40.0 °F
Cold impact resistance, breaks of 10, 454g; SAE J844
 0.000
@Temperature -40.0 °C
0.000
@Temperature -40.0 °F
Cold impact resistance, breaks of 10, 454g; Pretreatment: 2h boiling water; SAE J844
 0.000
@Temperature -40.0 °C
0.000
@Temperature -40.0 °F
Cold impact resistance, breaks of 10, 454g; Pretreatment: 24h 110°C; SAE J844
 0.000
@Temperature -40.0 °C
0.000
@Temperature -40.0 °F
Cold impact resistance, breaks of 10, 880g;
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
with pendulum, pipe; Tube dimension: OD x WT 8x1 mm; DIN 73378
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 62631-3-1
Dielectric Constant  2.90
@Frequency 1.00e+6 Hz
2.90
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 3.70
@Frequency 100 Hz
3.70
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 37.0 kV/mm940 kV/inAC, S20/P50; Sim. To IEC 60243-1
 38.0 kV/mm965 kV/inAC, S20/S20, t.; IEC 60243-1
Dissipation Factor  0.0320
@Frequency 1.00e+6 Hz
0.0320
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0520
@Frequency 100 Hz
0.0520
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.5 µm/m-°C
@Temperature 25.0 - 55.0 °C
50.3 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 25.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
Melting Point 176 °C349 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FISO 75-1/-2
Vicat Softening Point  145 °C
@Load 5.10 kg
293 °F
@Load 11.2 lb
50 K/h; ISO 306
 175 °C
@Load 1.02 kg
347 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 47.0 °C117 °FISO 11357-1/-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7918 / 325050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.