MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nylene® 724 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Dry as molded. Injection molding grade. Nylene 724 is the heat stabilized version of 721 which is a medium impact modified nylon for fast, easy molding. In addition to heat stabilization to prevent thermal degradation, parts molded from Nylene 724 have good impact strength right out of the mold without post conditioning. Stiffness is near that of unmodified nylon 6. Cylinder temperatures should be in the 450 - 500ºF range.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPaASTM D638
Elongation at Break 200 %ASTM D638
Flexural Modulus 2.10 GPaASTM D790
Izod Impact, Notched 1.60 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 245 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PN6C4U / 54228

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.