MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC/ABS 7710 NA Polycarbonate Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: EMERGE™ PC/ABS 7710 NA advanced resin is a high impact, ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It has superior processability for injection molding applications, excellent aesthetics and is available in custom colors.

Main Characteristics:

  • RoHS Compliant
Applications:
  • Electrical housings
  • Electrical equipment
  • Business equipment

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
 1.18 g/ccISO 1183/B
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 in/inISO 294-4
Melt Flow 11 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 13 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
 20 g/10 min
@Load 5.00 kg,
Temperature 240 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120
@Thickness 3.20 mm
Injection Molded; ASTM D785
Tensile Strength at Break 45.0 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
 48.3 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Tensile Strength, Yield 55.0 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
 60.0 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Elongation at Break 43 %
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
 65 %
@Thickness 3.20 mm
Injection Molded; ASTM D638
Elongation at Yield 3.8 %
@Thickness 3.20 mm
Injection Molded; ASTM D638
 3.8 %
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Tensile Modulus 2560 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/1
 2620 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Flexural Strength 96.5 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D790
Flexural Modulus 2690 MPaInjection Molded; ASTM D790
Izod Impact, Notched 200 J/m
@Temperature -18.0 °C
ASTM D256
 440 J/m
@Temperature -22.0 °C
ASTM D256
 480 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Temperature -30.0 °C
Injection Molded; ISO 180/A
 50.0 kJ/m²
@Temperature 23.0 °C
Injection Molded; ISO 180/A
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
Injection Molded; ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
Injection Molded; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmIEC 60093
Surface Resistance 5.20e+15 ohmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.86
@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
@Thickness 3.20 mm
in Oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
in Oil; IEC 60243-1
Dissipation Factor 0.0040
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM D696
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CUnannealed; ISO 75-2/B
 90.6 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CUnannealed; ISO 75-2/A
 79.4 °CUnannealed; ASTM D648
Vicat Softening Point 94.0 °CISO 306/B50
 104 °CASTM D1525
 104 °CISO 306/A120
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VB
@Thickness 2.00 mm
 5VA
@Thickness 2.50 mm
Oxygen Index 28 %ASTM D2863
Glow Wire Flammability Index 925 °C
@Thickness 1.50 mm
IEC 60695-2-12
 925 °C
@Thickness 2.00 mm
IEC 60695-2-12
 925 °C
@Thickness 2.50 mm
IEC 60695-2-12
 950 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 270 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Trinseo EMERGE™ PC/ABS 7700 NA Polycarbonate Resin
Lotte Advanced Materials Infino® NH-1027HF PC/ABS, Unreinforced FR
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Aclo Acculoy POL063L Polycarbonate PET Alloy

PTRINS9054 / 197550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.