MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Infino® NH-1027HF PC/ABS, Unreinforced FR
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 0.20 %
@Temperature 23.0 °C
0.20 %
@Temperature 73.4 °F
ASTM D570
Melt Flow 55 g/10 min
@Load 10.0 kg,
Temperature 220 °C
55 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 59.8 MPa8680 psi50 mm/min; ASTM D638
Flexural Strength 88.3 MPa12800 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.35 GPa341 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched 5.39 J/cm
@Thickness 3.17 mm
10.1 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 98.0 °C208 °FB/50; ISO R306
Flammability, UL94  HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
 V-2
@Thickness 1.20 - 3.00 mm
V-2
@Thickness 0.0472 - 0.118 in
 V-1
@Thickness 1.00 mm
V-1
@Thickness 0.0394 in
 V-0
@Thickness 1.20 - 3.00 mm
V-0
@Thickness 0.0472 - 0.118 in
 5VB
@Thickness 1.50 - 3.00 mm
5VB
@Thickness 0.0591 - 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® NH-1017D PC/ABS, Unreinforced FR
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Trinseo EMERGE™ PC/ABS 7700 NA Polycarbonate Resin
Lotte Advanced Materials Infino® NH-1021U PC/ABS
Lotte Advanced Materials Infino® NE-1030TV PC/ABS

PSAMSU835 / 146652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.