MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is available in both dark and light electrical Grey, other colors can be made upon request.

Benefits: The product offers a robust glow wire resistance, combined with enhanced processing behavior suitable for thin wall parts.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This product is ideally suited for power distribution applications such as MCB housing.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183/A
Water Absorption 1.0 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.010 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0080 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO/FDIS 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPaISO 527 Type 1A
 75.0 MPaASTM D638
Elongation at Break 3.0 %ISO 527 Type 1A
 3.0 %ASTM D638
Tensile Modulus 6400 MPaISO 527 Type 1A
Flexural Strength 130 MPaASTM D790
 136 MPaISO 178
Flexural Modulus 600 MPaISO 178
 5700 MPaASTM D790
Izod Impact, Notched 55.0 J/mASTM D256
Charpy Impact Unnotched 47.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 252 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75/Af
 145 °CASTM D648
Flammability, UL94 V-2
@Thickness 0.800 mm
1210
 V-2
@Thickness 1.60 mm
1210
 V-2
@Thickness 3.20 mm
1210
Oxygen Index 31 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 - 235 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone230-240°C
Mixing Zone245-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Starflam® PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Envalior Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond)
Domo TECHNYL® 2417IG PA66, 20% glass fiber, DRY
Domo TECHNYL® 2412GM05-D PA66, 38% glass fiber, DRY
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY

PRHOD799 / 138030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.