MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection molding

Available in: Asia Pacific

Product Applications: TECHNYL® 2412GHF6 is used in all sectors of industry, offering excellent combination between thermal stability and mechanical properties. This grade is widely used for: Hot water distributor pipe, Motor holder for boiler. This product is available in natural and black color and in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
0.80 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D786
Tensile Strength, Yield 200 MPa29000 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D638
Flexural Strength 300 MPa43500 psiASTM D790
Flexural Modulus 9.70 GPa1410 ksiASTM D790
Izod Impact, Notched 1.30 J/cm2.44 ft-lb/inASTM D265
Charpy Impact, Notched 1.35 J/cm²6.42 ft-lb/in²ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohm6.00e+14 ohmIEC 60093
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243
Dissipation Factor 0.0100.010IEC 60250
Comparative Tracking Index 350 V350 VSolution B; IEC 60112
 450 V450 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 262 °C504 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 252 °C486 °FASTM D648
Flammability, UL94 HB
@Thickness 0.800 - 3.20 mm
HB
@Thickness 0.0315 - 0.126 in
Oxygen Index 23 %23 %ISO 4589
Glow Wire Flammability Index 700 °C
@Thickness 1.60 mm
1290 °F
@Thickness 0.0630 in
IEC-60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 270 - 280 °C518 - 536 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, Conditioned
Domo TECHNYL® eXten D247 F Nylon 66 & 610
Domo TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, Conditioned
Domo TECHNYL® 2412GHF8 PA66, 40% glass fiber, Conditioned

PRHOD572 / 137803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.