MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot LITX® 66 Conductive Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: LITX 66 conductive additive for lithium-ion batteries balances the need for conductivity, ease of use and cost. It is manufactured in China and is supplied in granular form to simplify handling while preserving ease of dispersion. Due to its unique properties, LITX 66 conductive additive can be used as a drop-in replacement for conventional conductive additives. In some formulations, it can be used at lower loadings than conventional additives, which may enable improved energy density. This conductive additive is primarily used as a cathode additive, but it can also be used as anode additive. These attributes make it a suitable choice for all lithium-ion battery applications that require a balance between performance, quality and cost.

Performance features - Incorporating LITX 66 conductive additive into an electrode can:

  • Improve cycle life, energy and power
  • Simplify handling while maintaining dispersibility
  • Reduce cost
  • Reduce the amount of conductive additive required
Key applications - LITX 66 conductive additive is suitable for use in multiple lithium-ion battery applications:
  • Mobile electronic batteries
  • Electric and hybrid vehicles that feature lithium-ion batteries, including large transport vehicles like buses
  • Energy storage applications, including solar energy panels

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Surface Area 340 - 420 m²/g340 - 420 m²/gBET nitrogen; ASTM D6556
 
Descriptive Properties
Content<10 ppmTotal Co, Cr, Cu, Mn, Ni
 <15 ppmIron
OAN155-195 mL/100gASTM D-2414
Product Formgranules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT152 / 315887

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.