System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Wieland 1751 Wilaform Palladium
Categories:
Metal
;
Nonferrous Metal
;
Precious Metal
;
Palladium Alloy
Material Notes:
Approach-steady palladium alloy for nearly all purposes in decoration manufacturing
Applications: casting, chains, laminar decoration, pipes, tubing
Dental
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
11.0
g/cc
0.397
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Vickers
130
130
HV5; glowed
Thermal Properties
Metric
English
Comments
Melting Point
1150
-
1220
°C
2100
-
2230
°F
Solidus
1150
°C
2100
°F
Liquidus
1220
°C
2230
°F
Processing Properties
Metric
English
Comments
Processing Temperature
800.0
°C
1472
°F
Cuvette Temp
Casting Temperature
1320
-
1420
°C
2410
-
2590
°F
Component Elements Properties
Metric
English
Comments
Copper, Cu
10 %
10 %
Palladium, Pd
50 %
50 %
Silver, Ag
40 %
40 %
Descriptive Properties
Color
grey
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Indium Corp. Indalloy 215 Silver Solder Alloy
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer
Johnson Matthey Pallabraze™ 1225 Palladium Bearing Brazing Filler Metal
Lucas-Milhaupt Cerametil 716 Active Metal Brazing
NWIELAN83 / 19885
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.