MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wieland 1751 Wilaform Palladium
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: Approach-steady palladium alloy for nearly all purposes in decoration manufacturing

Applications: casting, chains, laminar decoration, pipes, tubing

Dental

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 130HV5; glowed
 
Thermal PropertiesOriginal ValueComments
Melting Point 1150 - 1220 °C
Solidus 1150 °C
Liquidus 1220 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1472 °FCuvette Temp
Casting Temperature 1320 - 1420 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 10 %
Palladium, Pd 50 %
Silver, Ag 40 %
 
Descriptive Properties
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Indium Corp. Indalloy 215 Silver Solder Alloy
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer
Johnson Matthey Pallabraze™ 1225 Palladium Bearing Brazing Filler Metal
Lucas-Milhaupt Cerametil 716 Active Metal Brazing

NWIELAN83 / 19885

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.