MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. The structures produced with TN 2020 and PVdC or PA allow radiation treatment and present low rates of water vapor and oxygen permeation, which together ensure a longer shelf life for the food packed in this film. Since it presents an exceptional weldability, this product meets the requirements for automatic or semi-automatic lines of cutting, welding, and/or packaging (with or without vacuum-packed process). Tritheva TN 2020 resin has excellent performance during the extrusion operation, thermal stability, and a low consumption of energy for its processing, rendering to package production a dimensional uniformity and excellent visual properties with high transparency and gloss that enhance the printing and surface finish of the packaging. This product complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1350, to contact with foodstuff.

Applications: Shrinkable packaging for food stuff, such as: cheese, meat, ham, salami and other processed meats. Packaging for frozen products.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1350
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.931 g/ccASTM D1505
Vinyl Acetate Content 8.0 - 9.0 %
Thickness 50.0 microns
Melt Index of Compound 1.7 - 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ASTM D2240
Tensile Strength at Break 19.0 MPaASTM D638
Tensile Strength, Yield 7.00 MPaASTM D638
Film Elongation at Break, MD 485 %ASTM D882
Film Elongation at Break, TD 725 %ASTM D882
Elongation at Break 700 %ASTM D638
Secant Modulus, MD 0.0670 GPa5%; ASTM D882
Secant Modulus, TD 0.0640 GPa5%; ASTM D882
Film Tensile Strength at Break, MD 25.0 MPaASTM D882
Film Tensile Strength at Break, TD 22.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 °CASTM D3418
Vicat Softening Point 79.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.8 %ASTM D1003
Gloss 140 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 150 °CPlasticizing Zone
 145 - 165 °CMixture Zone
Feed Temperature 135 - 140 °C
Adapter Temperature 165 - 185 °C
Blow-up Ratio (BUR) 3.0Recommended
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer
Braskem Evateno® 3019 PE EVA Foam Copolymer
Braskem CN8092 EVA Molding Copolymer
Braskem Evateno® HM 2528 EVA Hot Melt Copolymer

PDAX114 / 29539

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.