MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem Evateno® 3019 PE EVA Foam Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Evateno® 3019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. Evateno® 3019 PE is an easy processing and crosslinkable product with high compatibility with other thermoplastic and elastomeric resins, and inorganic fillers. It offers elasticity, high environmental stress cracking resistance (ESCR), flexibility, and fatigue resistance. Crosslinked and/or expanded parts form several applications including: compounds for the footwear (sole, insoles, etc), toys, and gifts industry; and blends with polyethylene for film production, hot-melt adhesives formulation, and modified asphalts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM-D1505 / ASTM-D792
ESCR 100% Igepal® >= 300 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
>= 300 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Vinyl Acetate Content 19 %19 %
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM-D2240
Hardness, Shore D 3030ASTM-D2240
 
Thermal PropertiesMetricEnglishComments
Melting Point 86.0 °C187 °FASTM-D3418
Vicat Softening Point 60.0 °C
@Load 1.02 kg
140 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Evateno® 8019 PE EVA Foam Copolymer
Braskem PN2021 EVA Foam Copolymer
Braskem VA2019A EVA Foam Copolymer
Braskem Evateno® HM 2528 EVA Hot Melt Copolymer
ExxonMobil Escorene® MV 02514 EVA Copolymer, Adhesive and Sealant Grade

PBRAS818 / 106664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.