MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Insulcast® 136 Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 136 is an easy to use epoxy casting/potting compound exhibiting excellent adhesion to metals, ceramics and most plastics. When properly cured with INSULCURE 11B, INSULCAST 136 will conform to the requirements of MIL-I-16923, Types B, C & D, and will not support fungusgrowth.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccUncured. Insulcure 11B
 0.970 g/cc0.970 g/ccUncured. Insulcure 9
 1.59 g/cc1.59 g/ccUncured. Insulcast 136
Viscosity 55 cP55 cPInsulcure 9; ASTM D2393
 700 cP700 cPInsulcure 11B; ASTM D2393
 25000 cP25000 cPInsulcure 11B; ASTM D2393
 30000 cP30000 cPInsulcure 9; ASTM D2393
 80000 cP80000 cPInsulcast 136; ASTM D2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787cured. Insulcure 9; ASTM D2240
 8989cured. Insulcure 11B; ASTM D2240
Tensile Strength 68.9 MPa10000 psicured. Insulcure 9; ASTM D638
 70.3 MPa10200 psicured. Insulcure 11B; ASTM D638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %Cured. Insulcure 11B; ASTM D638
 2.0 - 4.0 %2.0 - 4.0 %Cured. Insulcure 9; ASTM D638
Flexural Strength 107 MPa15500 psiCured. Insulcure 9; ASTM D790
 117 MPa17000 psiCured. Insulcure 11B; ASTM D790
Compressive Strength 103 MPa15000 psiCured. Insulcure 9; ASTM D695
 107 MPa15500 psiCured. Insulcure 11B; ASTM D695
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+16 ohm-cm5.00e+16 ohm-cmInsulcure 11B; ASTM D150
 5.00e+16 ohm-cm5.00e+16 ohm-cmInsulcure 9; ASTM D150
Dielectric Constant  4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
Insulcure 11B; ASTM D150
 4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
Insulcure 9; ASTM D150
Dielectric Strength 17.3 kV/mm440 kV/inInsulcure 11B; ASTM D149
 17.3 kV/mm440 kV/inInsulcure 9; ASTM D149
Dissipation Factor  0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
ASTM D150
 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FCured. Insulcure 11B
 40.0 µm/m-°C22.2 µin/in-°FCured. Insulcure 9
Thermal Conductivity 0.720 W/m-K5.00 BTU-in/hr-ft²-°FCured. Insulcure 11B
 0.720 W/m-K5.00 BTU-in/hr-ft²-°FCured. Insulcure 9
Maximum Service Temperature, Air 105 °C221 °FInsulcure 9
 155 °C311 °FInsulcure 11B
Heat Distortion Temperature 80.0 °C176 °FLoad Not Reported. Insulcure 9
 155 °C311 °FLoad Not Reported. Insulcure 11B
Shrinkage 0.20 %0.20 %Cured. Insulcure 9
 0.20 %0.20 %Cured. Insulcure 11B
 
Processing PropertiesMetricEnglishComments
Pot Life  30.0 min
@Temperature 25.0 °C
30.0 min
@Temperature 77.0 °F
Insulcure 9
 150 min
@Temperature 25.0 °C
150 min
@Temperature 77.0 °F
Insulcure 11B
Shelf Life 12.0 Month12.0 MonthInsulcast 136
 12.0 Month12.0 MonthInsulcure 11B
 12.0 Month12.0 MonthInsulcure 9
 
Descriptive Properties
ColorAmberUncured. Insulcure 9
 AmberUncured. Insulcure 11B
 BlackUncured. Insulcast 136
Mix Ratio by weight100:6-7Insulcast 136:Insulcure 9
 100:9-10Insulcast 136:Insulcure 11B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWIN9098 / 239608

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.