MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

INEOS Styrolution Polystyrol 495 F GR 2 PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss. High flow, Good balance of toughness and heat resistance. Applications: Injection molding, TV & office equipment components, Air conditioners, Water tanks for toilet flushing.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inISO 294-4
Melt Flow 9.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 74.0 MPa10700 psiISO 2039-1
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break 40 %40 %ISO 527
Elongation at Yield 1.5 %1.5 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Flexural Strength 40.0 MPa5800 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Izod Impact, Notched 1.80 J/cm3.37 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 13.0 J/cm²
@Temperature -30.0 °C
61.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant  2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
IEC 60250
 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.00040
@Frequency 100 Hz
0.00040
@Frequency 100 Hz
IEC 60250
 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C55.6 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C192 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  90.0 °C
@Load 5.10 kg
194 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 98.0 °C
@Load 1.02 kg
208 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 260 °C356 - 500 °FISO 294
Mold Temperature 10.0 - 60.0 °C50.0 - 140 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
ColorNatural
Commercial StatusEurope
Primary Processing TechniqueInjection Molding
Surface Gloss45Skalenteile

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution PS 495F HIPS
KKPC Kuhmo HI 450S High Gloss HIPS
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe)
Chi Mei Polyrex® PH-60 Polystyrene - High Impact

PBASG0632 / 132265

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.