MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 psf and is also available unsupported at 0.06 psf.

Features: Flexible cure cycle; Good lap shear performance at temperatures ranging from -67°F to 180°F; Good peel properties from -67°F to 180°F; Good tack to assist in adhesive joint assembly; Less than 1% volatile content; Suitable for bonding a wide range of substrates.
Applications: Aluminum to aluminum bonding; Sandwich bonding with a variety of skins and cores

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 0.000 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1.02 ksiFlatwise Tensile
Shear Strength 2.20 ksi
@Temperature 98.9 °C
Lap Shear
 3.50 ksi
@Temperature 21.1 °C
Lap Shear, Environmental Conditioning: 160°F 95% RH (1000 hrs)
 3.50 ksi
@Temperature 82.2 °C
Lap Shear
 4.50 ksi
@Temperature 48.9 °C
Lap Shear
 4.80 ksi
@Temperature 21.1 °C
Lap Shear
Peel Strength 12.0 pli
@Temperature 82.2 °C
Bell Peel, Environmental Conditioning: 160°F 95% RH (1000 hrs)
 16.0 pli
@Temperature 21.1 °C
Bell Peel
 17.0 pli
@Temperature 21.1 °C
Bell Peel
 25.0 pli
@Temperature 48.9 °C
Bell Peel
 26.0 pli
@Temperature 82.2 °C
Bell Peel
 31.0 pli
@Temperature 98.9 °C
Bell Peel
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Areal Weight (psf)0.06
Climbing Drum Peel (in-lb/3in)2270°F
 28120°F
 28180°F
 32210°F
Roll Width (in)49
Standard Roll (ft2)1075
SupportCotton Scrim

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 7668 Epoxy Resin
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Hexcel® Redux® 609 (0.04 psf) Adhesive film for bonding metallic and composite components
Huntsman Araldite GY 282 Bisphenol F Epoxy Resin
Hexcel® Redux® 319L High Performance Modified Epoxy Film Adhesive (0.036 psf)

PHEXC468 / 99287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.