Physical Properties | Metric | English | Comments |
---|
Volatiles | <= 1.5 % | <= 1.5 % |
| <= 1.5 % | <= 1.5 % |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength | 372 MPa | 54000 psi |
| 427 MPa | 62000 psi |
| 434 MPa | 63000 psi |
| 434 MPa | 63000 psi |
| 462 MPa | 67000 psi |
| 359 MPa @Temperature 177 °C | 52000 psi @Temperature 351 °F |
| 414 MPa @Temperature 177 °C | 60000 psi @Temperature 351 °F |
| 414 MPa @Temperature 24.0 °C | 60000 psi @Temperature 75.2 °F |
| 421 MPa @Temperature 177 °C | 61000 psi @Temperature 351 °F |
| 427 MPa @Temperature 177 °C | 62000 psi @Temperature 351 °F |
| 441 MPa @Temperature 177 °C | 64000 psi @Temperature 351 °F |
| 503 MPa @Temperature 24.0 °C | 73000 psi @Temperature 75.2 °F |
| 510 MPa @Temperature 24.0 °C | 74000 psi @Temperature 75.2 °F |
| 510 MPa @Temperature 24.0 °C | 74000 psi @Temperature 75.2 °F |
| 517 MPa @Temperature 24.0 °C | 75000 psi @Temperature 75.2 °F |
Tensile Modulus | 20.0 GPa | 2900 ksi |
| 23.4 GPa | 3390 ksi |
| 24.1 GPa | 3500 ksi |
| 24.1 GPa | 3500 ksi |
| 26.2 GPa | 3800 ksi |
| 19.3 GPa @Temperature 177 °C | 2800 ksi @Temperature 351 °F |
| 22.1 GPa @Temperature 24.0 °C | 3210 ksi @Temperature 75.2 °F |
| 23.4 GPa @Temperature 177 °C | 3390 ksi @Temperature 351 °F |
| 24.1 GPa @Temperature 177 °C | 3500 ksi @Temperature 351 °F |
| 24.1 GPa @Temperature 177 °C | 3500 ksi @Temperature 351 °F |
| 24.8 GPa @Temperature 177 °C | 3600 ksi @Temperature 351 °F |
| 26.2 GPa @Temperature 24.0 °C | 3800 ksi @Temperature 75.2 °F |
| 26.2 GPa @Temperature 24.0 °C | 3800 ksi @Temperature 75.2 °F |
| 26.2 GPa @Temperature 24.0 °C | 3800 ksi @Temperature 75.2 °F |
| 26.9 GPa @Temperature 24.0 °C | 3900 ksi @Temperature 75.2 °F |
Compressive Strength | 331 MPa | 48000 psi |
| 358 MPa | 51900 psi |
| 358 MPa | 51900 psi |
| 393 MPa | 57000 psi |
| 407 MPa | 59000 psi |
| 352 MPa @Temperature 177 °C | 51100 psi @Temperature 351 °F |
| 358 MPa @Temperature 177 °C | 51900 psi @Temperature 351 °F |
| 365 MPa @Temperature 177 °C | 52900 psi @Temperature 351 °F |
| 365 MPa @Temperature 177 °C | 52900 psi @Temperature 351 °F |
| 393 MPa @Temperature 177 °C | 57000 psi @Temperature 351 °F |
| 517 MPa @Temperature 24.0 °C | 75000 psi @Temperature 75.2 °F |
| 545 MPa @Temperature 24.0 °C | 79000 psi @Temperature 75.2 °F |
| 552 MPa @Temperature 24.0 °C | 80100 psi @Temperature 75.2 °F |
| 572 MPa @Temperature 24.0 °C | 83000 psi @Temperature 75.2 °F |
| 572 MPa @Temperature 24.0 °C | 83000 psi @Temperature 75.2 °F |
Compressive Modulus | 21.4 GPa | 3100 ksi |
| 26.2 GPa | 3800 ksi |
| 26.2 GPa | 3800 ksi |
| 26.9 GPa | 3900 ksi |
| 29.0 GPa | 4210 ksi |
| 22.8 GPa @Temperature 177 °C | 3310 ksi @Temperature 351 °F |
| 23.4 GPa @Temperature 24.0 °C | 3390 ksi @Temperature 75.2 °F |
| 25.5 GPa @Temperature 177 °C | 3700 ksi @Temperature 351 °F |
| 25.5 GPa @Temperature 177 °C | 3700 ksi @Temperature 351 °F |
| 26.2 GPa @Temperature 177 °C | 3800 ksi @Temperature 351 °F |
| 26.2 GPa @Temperature 177 °C | 3800 ksi @Temperature 351 °F |
| 27.6 GPa @Temperature 24.0 °C | 4000 ksi @Temperature 75.2 °F |
| 28.3 GPa @Temperature 24.0 °C | 4100 ksi @Temperature 75.2 °F |
| 29.0 GPa @Temperature 24.0 °C | 4210 ksi @Temperature 75.2 °F |
| 29.6 GPa @Temperature 24.0 °C | 4290 ksi @Temperature 75.2 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Maximum Service Temperature, Air | 177 °C | 350 °F |
|
Descriptive Properties |
---|
Climbing Drum Peel | 18 Nm/m |
| 19.9 Nm/m |
| 19.9 Nm/m |
| 20.3 Nm/m |
| 20.6 Nm/m |
| 20.9 Nm/m |
| 21.2 Nm/m |
| 23.1 Nm/m |
| 24.6 Nm/m |
| 38 Nm/m |
| 52.3 Nm/m |
| 53.8 Nm/m |
| 54.1 Nm/m |
| 60.8 Nm/m |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.