Resin cured Ethylene Propylene Terpolymer, 70-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated for applications involving water and steam. Applications: Recommended for use in steam raising plant and heat exchanger equipment. Water and steam resistance is superior to that of Sulphur or Peroxide cured variants. Not suitable for use with mineral or di-ester based lubricants. |