MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Precision Polymer Engineering E70I Ethylene Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Resin cured Ethylene Propylene Terpolymer, 70-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated for applications involving water and steam.

Applications: Recommended for use in steam raising plant and heat exchanger equipment. Water and steam resistance is superior to that of Sulphur or Peroxide cured variants. Not suitable for use with mineral or di-ester based lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474°IRHD; ASTM D1415
 8484°IRHD, +10 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 10.4 MPa1510 psi-20% change after 70 hours @ 150°C; ASTM D412
 13.0 MPa1890 psiASTM D412
Elongation at Break 120 %120 %-20% change after 70 hours @ 150°C; ASTM D412
 150 %150 %ASTM D412
Compression Set 15 %
@Temperature 150 °C,
Time 86400 sec
15 %
@Temperature 302 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °FNon-brittle after 3 minutes
 -30.0 °C-22.0 °F
Flash Point >= 200 °C>= 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering E60Q Ethylene Propylene Rubber
Lanxess Keltan® 9950C Ethylene-Propylene Rubber
Lanxess Keltan® 9650Q Ethylene-Propylene Rubber
Lanxess Keltan® 8570C Ethylene-Propylene Rubber
Lanxess Keltan® 8570 Ethylene-Propylene Rubber

PPRECI058 / 57782

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.