MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pyrotek S-1100 Compressible Insulation Board
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.

Applications

  • Reduction cell insulation
  • Trough covers
  • Back-up insulation

Advantages

  • Exceptional heat resistance
  • Low thermal conductivity
  • High mechanical strength
  • Not damaged by water
  • Excellent creep resistance
  • Dimensional stability

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.250 g/cc0.00903 lb/in³
Water Absorption at Saturation 5.5 %5.5 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 1.40 MPa203 psi
Compressive Strength 2.50 MPa363 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0440 W/m-K
@Temperature 20.0 °C
0.305 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 0.0810 W/m-K
@Temperature 400 °C
0.562 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.130 W/m-K
@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Maximum Service Temperature, Air 1100.5 °C2012.9 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elisto THERMOSTAR® LD 1000 Frame Press Insulation Material
Pyrotek Pyroboard™ S1300 Roller
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base
Pyrotek Pyrite N-14 Refractory Board

CPYRO094 / 1830

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.