MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyroboard™ S1300 Roller
Categories: Ceramic

Material Notes: Pyroboard™ S1300 was developed specifically for use in hotter zones of an annealing furnace.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.833 g/cc0.0301 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1.86 MPa270 psi
Flexural Strength 3.45 MPa500 psi
Compressive Strength 3.10 MPa450 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0677 W/m-K0.470 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1260 °C2300 °F
Shrinkage  3.5 %
@Temperature 982 °C
3.5 %
@Temperature 1800 °F
Thickness
 4.8 %
@Temperature 982 °C
4.8 %
@Temperature 1800 °F
Surface
 10.2 %
@Temperature 1204 °C
10.2 %
@Temperature 2199 °F
Surface
 10.6 %
@Temperature 1204 °C
10.6 %
@Temperature 2199 °F
Thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EREY99 Yttrium Oxide
MarkeTech Silica Aerogel
Elisto THERMOSTAR® LD 1000 Frame Press Insulation Material
Unifrax Excelfrax® 1800 Board Microporous Insulation
Sharadaa Ceramics Resin Bonded Slabs

CPYRO212 / 1929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.