Physical Properties | Original Value | Comments |
---|
Specific Gravity | 1.20 g/cc |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Shore A | 71 |
| 58 @Treatment Temp. 23.0 °C, Time 252000 sec |
| 61 @Treatment Temp. 23.0 °C, Time 252000 sec |
| 65 @Treatment Temp. 125 °C, Time 252000 sec |
| 65 @Treatment Temp. 150 °C, Time 252000 sec |
| 66 @Treatment Temp. 100 °C, Time 252000 sec |
| 71 @Treatment Temp. 100 °C, Time 252000 sec |
| 71 @Treatment Temp. 23.0 °C, Time 252000 sec |
| 73 @Treatment Temp. 150 °C, Time 252000 sec |
| 73 @Treatment Temp. 100 °C, Time 252000 sec |
| 73 @Treatment Temp. 125 °C, Time 252000 sec |
| 75 @Treatment Temp. 100 °C, Time 252000 sec |
| 77 @Treatment Temp. 125 °C, Time 252000 sec |
| 77 @Treatment Temp. 100 °C, Time 252000 sec |
| 81 @Treatment Temp. 100 °C, Time 252000 sec |
| 81 @Treatment Temp. 150 °C, Time 252000 sec |
Tensile Strength | 2993 psi |
| 56.6 psi @Treatment Temp. 23.0 °C, Time 252000 sec |
| 1248.1 psi @Treatment Temp. 23.0 °C, Time 252000 sec |
| 1762.9 psi @Treatment Temp. 23.0 °C, Time 252000 sec |
| 2319.9 psi @Treatment Temp. 125 °C, Time 252000 sec |
| 2523.1 psi @Treatment Temp. 100 °C, Time 252000 sec |
| 2523.1 psi @Treatment Temp. 150 °C, Time 252000 sec |
| 2885.3 psi @Treatment Temp. 150 °C, Time 252000 sec |
| 3004.9 psi @Treatment Temp. 125 °C, Time 252000 sec |
| 3013.9 psi @Treatment Temp. 100 °C, Time 252000 sec |
| 3034.9 psi @Treatment Temp. 100 °C, Time 252000 sec |
| 3085.8 psi @Treatment Temp. 100 °C, Time 252000 sec |
| 3109.7 psi @Treatment Temp. 125 °C, Time 252000 sec |
| 3109.7 psi @Treatment Temp. 100 °C, Time 252000 sec |
| 3124.7 psi @Treatment Temp. 150 °C, Time 252000 sec |
Elongation, Ultimate | 307 % |
| 146.1 % @Treatment Temp. 23.0 °C, Time 252000 sec |
| 206 % @Treatment Temp. 23.0 °C, Time 252000 sec |
| 264.9 % @Treatment Temp. 150 °C, Time 252000 sec |
| 264.9 % @Treatment Temp. 100 °C, Time 252000 sec |
| 307 % @Treatment Temp. 100 °C, Time 252000 sec |
| 307 % @Treatment Temp. 125 °C, Time 252000 sec |
| 310.07 % @Treatment Temp. 23.0 °C, Time 252000 sec |
| 311.9 % @Treatment Temp. 100 °C, Time 252000 sec |
| 318.1 % @Treatment Temp. 125 °C, Time 252000 sec |
| 337.1 % @Treatment Temp. 100 °C, Time 252000 sec |
| 337.1 % @Treatment Temp. 100 °C, Time 252000 sec |
| 337.1 % @Treatment Temp. 125 °C, Time 252000 sec |
| 337.1 % @Treatment Temp. 150 °C, Time 252000 sec |
| 338.9 % @Treatment Temp. 150 °C, Time 252000 sec |
100% Modulus | 594 psi |
Tear Strength | 233 pli |
| 293 pli |
Compression Set | 11.5 % @Treatment Temp. 100 °C, Time 79200 sec |
| 11.6 % @Treatment Temp. 125 °C, Time 79200 sec |
| 11.6 % @Treatment Temp. 100 °C, Time 79200 sec |
| 12.6 % @Treatment Temp. 125 °C, Time 79200 sec |
| 15 % @Treatment Temp. 100 °C, Time 252000 sec |
| 15.2 % @Treatment Temp. 150 °C, Time 79200 sec |
| 16 % @Treatment Temp. 100 °C, Time 252000 sec |
| 16.6 % @Treatment Temp. 150 °C, Time 79200 sec |
|
Thermal Properties | Original Value | Comments |
---|
Brittleness Temperature | -38.0 °F |
Shrinkage | -3.70 % @Treatment Temp. 150 °C, Time 252000 sec |
| -3.60 % @Treatment Temp. 125 °C, Time 252000 sec |
| -3.40 % @Treatment Temp. 100 °C, Time 252000 sec |
| 0.30 % @Treatment Temp. 100 °C, Time 252000 sec |
| 4.1 % @Treatment Temp. 23.0 °C, Time 252000 sec |
| 12.5 % @Treatment Temp. 100 °C, Time 252000 sec |
| 12.9 % @Treatment Temp. 125 °C, Time 252000 sec |
| 14 % @Treatment Temp. 150 °C, Time 252000 sec |
| 36.7 % @Treatment Temp. 23.0 °C, Time 252000 sec |
| 58.6 % @Treatment Temp. 23.0 °C, Time 252000 sec |
|
Descriptive Properties |
---|
Color | Black |