MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.

Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkage temperature.

Processing characteristics of Elvaloy® 3108 AC are similar to LDPE and conventional polyethylene extruders are recommended.

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D792 - ISO 1183
Thickness 40.0 microns
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238 - ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 8.00 MPa500 mm/min; ISO 527-3
Film Tensile Strength at Yield, TD 7.00 MPa500 mm/min; ISO 527-3
Film Elongation at Break, MD 200 %500 mm/min; ISO 527-3
Film Elongation at Break, TD 600 %500 mm/min; ISO 527-3
Coefficient of Friction, Dynamic 0.15MD; ISO 8295
Elmendorf Tear Strength, MD 0.0250 g/micronISO 6383/2
Elmendorf Tear Strength, TD 0.0250 g/micronISO 6383/2
Dart Drop 7.50 g/micronISO 7765/1A
Film Tensile Strength at Break, MD 24.0 MPa500 mm/min; ISO 527-3
Film Tensile Strength at Break, TD 18.0 MPa500 mm/min; ISO 527-3
 
Optical PropertiesOriginal ValueComments
Haze 16 %ASTM D1003
Gloss 60 %ASTM D2457
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 150 °CExtrusion lamination and extrusion coating
 150 °CCast film
 150 °CBlown film
Middle Barrel Temperature 160 °CBlown film
 210 °CCast film
 220 °CExtrusion lamination
Front Barrel Temperature 170 °CBlown film
 250 °CCast film
 290 °CExtrusion lamination
Adapter Temperature 180 °CBlown film
 250 °CCast Film
 290 °CExtrusion lamination
Die Temperature 356 °FBlown film
 482 °FCast film
 554 °FExtrusion lamination
Blow-up Ratio (BUR) 2.0for 40 micron film
 
Descriptive Properties
BA-Content7 wt.%DuPont Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin
Dow Elvaloy® HP441 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer

PDUPM067 / 33734

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.