MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.

Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkage temperature.

Processing characteristics of Elvaloy® 3108 AC are similar to LDPE and conventional polyethylene extruders are recommended.

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D792 - ISO 1183
Thickness 40.0 microns1.57 mil
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.00 MPa1160 psi500 mm/min; ISO 527-3
Film Tensile Strength at Yield, TD 7.00 MPa1020 psi500 mm/min; ISO 527-3
Film Elongation at Break, MD 200 %200 %500 mm/min; ISO 527-3
Film Elongation at Break, TD 600 %600 %500 mm/min; ISO 527-3
Coefficient of Friction, Dynamic 0.150.15MD; ISO 8295
Elmendorf Tear Strength, MD 0.0250 g/micron0.635 g/milISO 6383/2
Elmendorf Tear Strength, TD 0.0250 g/micron0.635 g/milISO 6383/2
Dart Drop 7.50 g/micron191 g/milISO 7765/1A
Film Tensile Strength at Break, MD 24.0 MPa3480 psi500 mm/min; ISO 527-3
Film Tensile Strength at Break, TD 18.0 MPa2610 psi500 mm/min; ISO 527-3
 
Optical PropertiesMetricEnglishComments
Haze 16 %16 %ASTM D1003
Gloss 60 %60 %ASTM D2457
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 150 °C302 °FExtrusion lamination and extrusion coating
 150 °C302 °FCast film
 150 °C302 °FBlown film
Middle Barrel Temperature 160 °C320 °FBlown film
 210 °C410 °FCast film
 220 °C428 °FExtrusion lamination
Front Barrel Temperature 170 °C338 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Adapter Temperature 180 °C356 °FBlown film
 250 °C482 °FCast Film
 290 °C554 °FExtrusion lamination
Die Temperature 180 °C356 °FBlown film
 250 °C482 °FCast film
 290 °C554 °FExtrusion lamination
Blow-up Ratio (BUR) 2.02.0for 40 micron film
 
Descriptive Properties
BA-Content7 wt.%DuPont Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin
Dow Elvaloy® HP441 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer

PDUPM067 / 33734

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.