MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Morbond AL Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Bauxite raw material base. Chemical bond. Morbond AL is a two component system that forms a rapid setting, easily placed castable on mixing, which can be brought quickly into service. It is a bauxite based composition specifically developed for aluminium contact applications, exhibiting excellent resistance to corundum growth and metal penetration. Applications: Suitable repair material for metal contact areas in aluminium re-heat and holding furnaces.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.65 g/cc0.0957 lb/in³dried to 110°C
Grain Size <= 4000 µm<= 4000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  30.0 MPa
@Treatment Temp. 110 °C
4350 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 30.0 MPa
@Treatment Temp. 815 °C
4350 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 30.0 MPa
@Treatment Temp. 1000 °C
4350 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 30.0 MPa
@Treatment Temp. 1450 °C
4350 psi
@Treatment Temp. 2640 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.42 W/m-K
@Temperature 600 °C
16.8 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1450 °C<= 2640 °F
Shrinkage  0.10 %
@Treatment Temp. 815 °C
0.10 %
@Treatment Temp. 1500 °F
 0.10 %
@Treatment Temp. 1000 °C
0.10 %
@Treatment Temp. 1830 °F
 1.0 %
@Treatment Temp. 1450 °C
1.0 %
@Treatment Temp. 2640 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 87 %87 %
CaO 1.6 %1.6 %
Fe2O3 0.60 %0.60 %
K2O+Na2O 0.20 %0.20 %Na2O+ K2O
MgO 0.10 %0.10 %
P2O5 5.4 %5.4 %
SiO2 3.0 %3.0 %
TiO2 1.6 %1.6 %
 
Descriptive Properties
Net Material Required (kg/m³)2650
Water Additionaccelerator, 1 bottle, 25 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6266 / 203050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.