MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EB502 12.5% EVA Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sealing characteristics. This resin has excellent low temperature brittleness properties, melt strength, and flexibility. This resin grade complies with 21 CFR 177.1350. Melt temperatures of 360° F – 390° F are recommended. Test specimens for blown film: nominal thickness 2.0 mils; blow up ratio 2.5:1; die gap 35 mils.

Key Words: Excellent toughness and good heat sealing characteristics. 12.5% EVA.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccASTM-D1505
Melt Flow 0.55 g/10 minASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %ASTM-D882
Film Elongation at Break, TD 950 %ASTM-D882
Dart Drop 290 g/milASTM-D1709
Dart Drop Test 580 gASTM-D1709
Film Tensile Strength at Break, MD 27.6 MPaASTM-D882
Film Tensile Strength at Break, TD 29.6 MPaASTM-D882
1% Secant Modulus, MD 11000 psiASTM-D882
1% Secant Modulus, TD 13000 psiASTM-D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 94.0 °CPeak DSC; ASTM D-3418
Vicat Softening Point 76.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %ASTM-D1003
Gloss 70 %Specular; Angle 45°; ASTM-D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 390 °FBUR > 1.5:1
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Micropol E188 Rotational molding powder based on a random EVA copolymer
Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer
Westlake Elevate™ EB591 9% EVA Copolymer
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate

PWESF9043 / 130350

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.