MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kolon ELLAS K-260D Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Applications
  • Extrusion: Antenna, Heel Tip
  • Injection: Hose, Tube, Sheet
  • Industry Parts

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength 550 kg(f)/cm²ASTM D412
Tensile Stress at Strain 160 kg(f)/cm²
@Strain 100 %
ASTM D412
Elongation at Break 440 %ASTM D412
Tear Strength 180 kg(f)/cmASTM D624
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 195 - 205 °CInjection Molding
Zone 1 160 - 175 °CInjection Molding
 160 - 175 °CExtrusion Molding
Zone 2 180 - 190 °CInjection Molding
 180 - 195 °CExtrusion Molding
Zone 3 180 - 195 °CExtrusion Molding
 185 - 195 °CInjection Molding
Zone 4 190 - 205 °CExtrusion Molding
Die Temperature 190 - 205 °CExtrusion Molding
Head Temperature 195 - 210 °CExtrusion Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® AC-4095A TPU – Clear Aromatic
Lubrizol LifeSciences Carbothane® PC-3555D TPU – Clear Aliphatic
Lubrizol LifeSciences Carbothane® AC-4055D TPU – Clear Aromatic
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane

PKOKZ981 / 122683

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.