MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sibur SKS-30 ARKPN 1st Group Styrene-Butadiene Rubber (SBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SBR-1502. For use in the tire industry for production of tire thread and other parts for tires, in rubber technical industry for production of a wide assortment of rubber technical articles, and in the shoe industry for production of white and colored rubber footwear.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 27 - 37
@Temperature 100 °C
ML 1-4
Ash <= 0.80 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22 - 25 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 23.0 MPa
Elongation at Break >= 560 %
 
Descriptive Properties
Loss During Drying<0.4%
Mass Share Adigol-20.7-1.2%
Mass Share of A-Methyl Styrene22-25%
Mass Share of P-230.4-1.2%
Mass Share of VS-30A1-2%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sibur SKS-30 ARK 2nd Grade Styrene-Butadiene Rubber (SBR)
Cri-Tech LS-715 FKM Fluoroelastomer, Durometer 70A
Armacell Monarch® F-05013 (Black) Neoprene, EPDM, SBR Blend Foam
ATG s.r.l. SBR Styrene-Butadiene Rubber
Dow BETAPHON™ 2 Synthetic Rubber

PSIB094 / 67657

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.