MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow BETAPHON™ 2 Synthetic Rubber  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: BETAPHON™ 2 is an extrudable vibration damping coating. It can be applied robotically to oily metal panels in critical areas where high vibration damping is required, such as doors or roofs. It offers an automated alternative in the body shop or stamping plant to manually applied damping pads.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content >= 99 %>= 99 %3 hr @ 105°C
Viscosity Measurement  20
@Temperature 23.0 °C
20
@Temperature 73.4 °F
[g/min] Extruding Viscosity (Severs/Press flow; 5mm orifice, @ 43 psi)
 70
@Temperature 45.0 °C
70
@Temperature 113 °F
[g/min] Extruding Viscosity (Severs/Press flow; 5mm orifice, @ 43 psi)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 220 °C428 °F30 min
 
Descriptive Properties
Damping Performance: Composite Loss Factor0.192SAE J 1637, 2 mm thick, 10°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
KKPC KOSYN 1507H Styrene Butadiene Rubber
KKPC KOSYN 1500 Styrene Butadiene Rubber
Armacell Monarch® F-05013 (Black) Neoprene, EPDM, SBR Blend Foam
ATG s.r.l. SBR Styrene-Butadiene Rubber
Cri-Tech LS-715 FKM Fluoroelastomer, Durometer 70A

PDOW1132 / 30336

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.