MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) and cold isostatic pressing (CIP) followed by extrusion or sheet rolling processes. The material is also available as an investment casting under the name AlBeCast™.

Used for heat sinks and structural parts in aircraft and satellite avionics because of its low density, high modulus, high thermal conductivity, low CTE, thermal stability and isotropic properties.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: Aluminum Beryllium Composite Alloy AM162
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.071 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 262 MPa
 307 MPaTypical
Tensile Strength, Yield >= 193 MPa
 226 MPaTypical
Elongation at Break >= 2.0 %
 5.0 %Typical
Modulus of Elasticity 193 GPa
Poissons Ratio 0.17
Shear Modulus 82.0 GPacalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000350 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.91 µm/m-°C
@Temperature 25.0 °C
Specific Heat Capacity 1.56 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 210 W/m-K
Melting Point 1082 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 38 %As remainder
Beryllium, Be 60 - 64 %
Carbon, C <= 0.10 %
Other, each <= 0.20 %
Oxygen, O <= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Materion AlBeCast™ IC910 Aluminum Beryllium Composite
Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite
Aluminum - SiC Metal Matrix Composite

NBB000 / 15086

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.