MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Lord Adhesives CoolTherm™ EP-6007/6010 Epoxy System, EP-6007 BLK Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD CoolTherm™ EP-6007 BLK resin is a ceramic filled epoxy resin specifically formulated for use with CoolTherm or Thermoset™ hardeners to create a two component system. This system is recommended for use as a thermally conductive, thin bondline adhesive for attaching semiconductors to heat sinks, and as a low viscosity potting and casting product for applications where thermal conductivity and non-burning properties are required.

Features: provides high thermal conductivity for applications where superior heat transfer is required. provides excellent high voltage insulation. exhibits low exotherm heat rise during room temperature cure. can be used on parts and devices that experience operating temperatures from -55°C to +130°C. provides excellent flame retardancy; UL 94 V-0 certified; meets requirements of Military Specifications MIL T-27 and MIL I-16923.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption  0.40 %
@Temperature 25.0 °C,
Time 864000 sec
0.40 %
@Temperature 77.0 °F,
Time 240 hour
cured, CoolTherm-6010 Hardener
 0.40 %
@Temperature 25.0 °C,
Time 864000 sec
0.40 %
@Temperature 77.0 °F,
Time 240 hour
cured, Thermoset Hardener No. 67
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/incured, CoolTherm-6010 Hardener
 0.0030 cm/cm0.0030 in/incured, Thermoset Hardener No. 67
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585cured, CoolTherm-6010 Hardener
 8585cured, Thermoset Hardener No. 67
Tensile Strength  57.9 MPa
@Temperature 25.0 °C
8400 psi
@Temperature 77.0 °F
cured, CoolTherm-6010 Hardener
 67.6 MPa
@Temperature 25.0 °C
9800 psi
@Temperature 77.0 °F
cured, Thermoset Hardener No. 67
Elongation at Yield 0.70 %0.70 %cured, CoolTherm-6010 Hardener
 1.2 %1.2 %cured, Thermoset Hardener No. 67
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  2.00e+16 ohm-cm
@Temperature 25.0 °C
2.00e+16 ohm-cm
@Temperature 77.0 °F
cured, CoolTherm-6010 Hardener
 2.00e+16 ohm-cm
@Temperature 25.0 °C
2.00e+16 ohm-cm
@Temperature 77.0 °F
cured, Thermoset Hardener No. 67
Dielectric Constant  4.3
@Frequency 100000 Hz,
Temperature 25.0 °C
4.3
@Frequency 100000 Hz,
Temperature 77.0 °F
cured, CoolTherm-6010 Hardener
 4.4
@Frequency 100000 Hz,
Temperature 25.0 °C
4.4
@Frequency 100000 Hz,
Temperature 77.0 °F
cured, Thermoset Hardener No. 67
Dielectric Strength 19.3 kV/mm490 kV/in
 19.7 kV/mm500 kV/in
Dissipation Factor  0.020
@Frequency 100000 Hz,
Temperature 25.0 °C
0.020
@Frequency 100000 Hz,
Temperature 77.0 °F
cured, CoolTherm-6010 Hardener
 0.020
@Frequency 100000 Hz,
Temperature 25.0 °C
0.020
@Frequency 100000 Hz,
Temperature 77.0 °F
cured, Thermoset Hardener No. 67
 
Thermal PropertiesMetricEnglishComments
CTE, linear 42.0 µm/m-°C23.3 µin/in-°Fcured, Thermoset Hardener No. 67, alpha 1
 47.0 µm/m-°C26.1 µin/in-°Fcured, CoolTherm-6010 Hardener, alpha 1
 122 µm/m-°C67.8 µin/in-°Fcured, CoolTherm-6010 Hardener, alpha 2
 140 µm/m-°C77.8 µin/in-°Fcured, Thermoset Hardener No. 67, alpha 2
Thermal Conductivity 0.500 W/m-K3.47 BTU-in/hr-ft²-°Fcured, Thermoset Hardener No. 67
 0.600 W/m-K4.16 BTU-in/hr-ft²-°Fcured, CoolTherm-6010 Hardener
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 54.0 °C129 °Fcured, CoolTherm-6010 Hardener, by TMA
 94.0 °C201 °Fcured, Thermoset Hardener No. 67, by TMA
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  180 min
@Temperature 130 °C
3.00 hour
@Temperature 266 °F
with Thermoset Hardener No. 67, suitable for pourings of up to 227 grams in a concentrate mass
 300 min
@Temperature 100 °C
5.00 hour
@Temperature 212 °F
with Thermoset Hardener No. 67, suitable for pourings of up to 227 grams in a concentrate mass
 720 - 960 min
@Temperature 25.0 °C
12.0 - 16.0 hour
@Temperature 77.0 °F
with CoolTherm EP-6010 Hardener
 960 min
@Temperature 65.0 °C
16.0 hour
@Temperature 149 °F
with Thermoset Hardener No. 67, suitable for pourings of up to 227 grams in a concentrate mass
Pot Life  2.00 min
@Temperature 25.0 °C
2.00 min
@Temperature 77.0 °F
with CoolTherm EP-6010 Hardener
 8.00 min
@Temperature 25.0 °C
8.00 min
@Temperature 77.0 °F
with Thermoset Hardener No. 67
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
from date of manufacture in original, unopened container
 
Descriptive Properties
AppearanceBlack Liquid
Mix Ratio100 to 5.5by weight, resin to hardener, CoolTherm EP-6010 Hardener
 100 to 9by weight, resin to hardener, Thermoset Hardener No. 67

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECASINT™ 2011 Polyimide (PI)
Overview of materials for Polyester (Thermoset) - Rigid
Rogers Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System
Precision Polymer Engineering N80C Nitrile Rubber
Precision Polymer Engineering N70C Nitrile Rubber

PLORD9162 / 232550

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.