MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.

Key features and benefits are:

  • Non-Halogen FR technology for regulatory compliance
  • Excellent dimensional stability and electrical properties
  • Recognized by Underwriter's Laboratories, File #E42524
  • Outstanding flow and fill in compression, transfer and injection molding.
  • Pigmentable for molded-in color, best appearance with mold texture
  • Designed for compression, transfer or injection molding in matched metal die molds.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 1.95 g/cc1.80 - 1.95 g/cc
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm0.0015 - 0.0030 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 33.0 MPa4790 psiASTM D638
Tensile Modulus 12.0 GPa1740 ksiASTM D638
Flexural Strength 79.0 MPa11500 psiASTM D790
Flexural Modulus 8.30 GPa1200 ksiASTM D790
Poissons Ratio 0.300.30
Shear Modulus 4.60 GPa667 ksiCalculated
Izod Impact, Notched 1.85 J/cm3.47 ft-lb/inASTM D256
Izod Impact, Unnotched 3.20 J/cm5.99 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm457 kV/inASTM D149
Arc Resistance 220 sec220 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FASTM D792
UL RTI, Electrical 130 °C266 °FUL 746C
UL RTI, Mechanical with Impact 130 °C266 °FUL 746C
UL RTI, Mechanical without Impact 130 °C266 °FUL 746C
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 5VB
@Thickness 2.60 mm
5VB
@Thickness 0.102 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression, Transfer or Injection Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polynt BMC 1150 Bulk Molding Compound ARC Ablation
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
Plenco PlasGlas™ 40118 High Strength Glass Filled Thermoset Polyester BMC
Polynt 30 CF60- 6mm Carbon Fiber VE BMC
Polynt BMC 1151 GRIGIO Bulk Molding Compound ARC Ablation

PPREMH970 / 140368

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.