MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Easy flow, glossy, impact resistant.

Applications: General purpose
Various technical parts, household appliances, hobby and office equipment, etc.

Synthos was formerly known as Kaucuk. All information provided by Synthos.

Key Words: ABS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inInternal; 50x50mm
Melt Flow 21 g/10 min
@Load 10.0 kg,
Temperature 220 °C
21 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Granulate; ISO 1133/U
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 97.0 MPa14100 psiH 358/30; Ø 50x4mm; ISO 2039-1
Tensile Strength at Break 30.0 MPa
@Temperature 23.0 °C
4350 psi
@Temperature 73.4 °F
50mm/min; ISO 527-2/1A/50
Tensile Strength, Yield 38.0 MPa
@Temperature 23.0 °C
5510 psi
@Temperature 73.4 °F
50mm/min; ISO 527-2/1A/50
Elongation at Break 10 %10 %50mm/min; ISO 527-2/1A/50
Tensile Modulus 2.30 GPa
@Temperature 23.0 °C
334 ksi
@Temperature 73.4 °F
1mm/min; ISO 527-2/1A/1
Flexural Strength 60.0 MPa
@Temperature 23.0 °C
8700 psi
@Temperature 73.4 °F
2mm/min; 80x10x4mm; ISO 178
Flexural Modulus 2.10 GPa
@Temperature 23.0 °C
305 ksi
@Temperature 73.4 °F
2mm/min; 80x10x4mm; ISO 178
Izod Impact, Notched (ISO) 24.0 kJ/m²
@Temperature 23.0 °C
11.4 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 180/1A
Charpy Impact Unnotched 17.0 J/cm²
@Temperature 23.0 °C
80.9 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm4.00e+16 ohm-cm500V; Ø 93x3mm; IEC 60093
Surface Resistance 2.00e+16 ohm2.00e+16 ohm500V; Ø 93x3mm; IEC 60093
Dielectric Constant  <= 2.7
@Frequency 50 Hz
<= 2.7
@Frequency 50 Hz
Ø 50x3mm; IEC 60250
 2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
Ø 50x3mm; IEC 60250
Dielectric Strength  13.0 kV/mm
@Thickness 3.00 mm
330 kV/in
@Thickness 0.118 in
Transformer Oil; IEC 60243-1
 57.0 kV/mm
@Thickness 0.500 mm
1450 kV/in
@Thickness 0.0197 in
Transformer Oil; IEC 60243-1
Dissipation Factor  0.0040
@Frequency 50 Hz
0.0040
@Frequency 50 Hz
Ø 93x3mm; IEC 60250
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
Ø 93x3mm; IEC 60250
Arc Resistance 89 sec89 secØ 93x3mm; IEC 61621
Comparative Tracking Index 400 V400 VSolution A; Ø 93x3mm; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C210 °F80x10x4mm; ISO 75-2/Af
Vicat Softening Point 95.0 °C203 °F50°C/h; 50N; 10x10x4mm; ISO 306/B50
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Tested in EZÚ Praha
Glow Wire Test 650 °C1200 °FØ 93x3mm; IEC 60695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SEKISUI SPI ALLEN® 6000 PMMA/ABS
Trinseo Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® LGA Acrylonitrile Butadiene Styrene (ABS)
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Ineos Nova PS9410 High Impact Polystyrene

PSYNT025 / 82638

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.