MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
European Plane Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)
Common Applications: Decorative purposes. Inlay work

Key Words: Platanus Hybrida; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.630 g/ccAir Dry (12-15% Moisture Content)
Cell Length 1.40 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4800 NSide
Tensile Strength, Ultimate 5.20 MPaPerpendicular to Grain
Modulus of Rupture 0.0970 GPaStatic Bending
Flexural Modulus 10.29 GPaStatic Bending
Compressive Strength 6.40 MPaPerpendicular to Grain
 45.0 MPaParallel to Grain
Machinability 50 %Medium Relative to Other Wood
Shear Strength 9.80 MPaOrientation Unknown
Toughness 27.6 J2 cm x 2 cm sample
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.50 %Axial; Green to Zero Moisture
 4.5 %Radial; Green to Zero Moisture
 8.7 %Tangential; Green to Zero Moisture
 13.7 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorMottled red-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
European White Oak Wood
European Hornbeam Wood
European Oak Wood
European Poplar Wood
European Red Oak Wood

PTSE090 / 71318

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.