MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

European White Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Key Words: Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 - 0.450 g/cc0.0116 - 0.0163 lb/in³Earlywood
 0.890 - 0.930 g/cc0.0322 - 0.0336 lb/in³Latewood
Cell Length 1.20 mm0.0472 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 5500 N1240 lb (f)Side
Tensile Strength, Ultimate 3.00 MPa435 psiPerpendicular to Grain
 109 MPa15800 psiAxial
Modulus of Rupture 0.0910 GPa13.2 ksiStatic Bending
Flexural Modulus 12.25 GPa1777 ksiStatic Bending
Compressive Strength 7.80 MPa1130 psiPerpendicular to Grain
 43.0 MPa6240 psiParallel to Grain
Shear Strength 11.6 MPa1680 psiOrientation Unknown
Toughness 29.6 J21.8 ft-lb2 cm x 2 cm sample
Cleavage 9.00 kN/m51.4 lb/in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.10 - 0.40 %0.10 - 0.40 %Axial; Green to Zero Moisture
 3.9 - 6.5 %3.9 - 6.5 %Radial; Green to Zero Moisture
 7.8 - 13.8 %7.8 - 13.8 %Tangential; Green to Zero Moisture
 11.8 - 19 %11.8 - 19 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
European Oak Wood
European Red Oak Wood
American White Oak Wood
European Walnut Wood
European Ash Wood

PTSE130 / 71322

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.