MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory developed Custom 455® stainless, a martensitic age-hardenable stainless steel. This alloy is relatively soft and formable in the annealed condition. A single-step aging treatment develops exceptionally high yield strength with good ductility and toughness. This stainless can be machined in the annealed condition, and welded in much the same manner as other precipitation hardenable stainless steels. Because of its low work-hardening rate, it can be extensively cold formed. The dimensional change during hardening is only about -0.001 in/in, which permits close-tolerance finish machining in the annealed state. Custom 455 stainless represents a significant advancement in the area of precipitation hardening stainless steels. It should be considered where simplicity of heat treatment, ease of fabrication, high strength and corrosion resistance are required in combination.

Because of the unique combination of high strength and corrosion resistance of Custom 455 stainless there are few other alloys available for consideration. Carpenter PH13-8 Mo can be considered where good transverse toughness and ductility are necessary in large sections.

Custom 455® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS S45500
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.76 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 411411Estimated from Rockwell C for 3000 kg load, 10 mm ball Brinell measurement.
Hardness, Knoop 450450Estimated from Rockwell C
Hardness, Rockwell C 4444
Hardness, Vickers 430430Estimated from Rockwell C
Tensile Strength, Ultimate 1413 MPa204900 psi
 814 MPa
@Temperature 538 °C
118000 psi
@Temperature 1000 °F
 1062 MPa
@Temperature 427 °C
154000 psi
@Temperature 801 °F
 1200 MPa
@Temperature 316 °C
174000 psi
@Temperature 601 °F
 1517 MPa
@Temperature -73.0 °C
220000 psi
@Temperature -99.4 °F
 1758 MPa
@Temperature -184 °C
255000 psi
@Temperature -299 °F
Tensile Strength, Yield 1345 MPa
@Strain 0.2 %
195100 psi
@Strain 0.2 %
 138 MPa
@Strain 0.2 %,
Temperature 316 °C
20000 psi
@Strain 0.2 %,
Temperature 601 °F
 738 MPa
@Strain 0.2 %,
Temperature 538 °C
107000 psi
@Strain 0.2 %,
Temperature 1000 °F
 1020 MPa
@Strain 0.2 %,
Temperature 427 °C
148000 psi
@Strain 0.2 %,
Temperature 801 °F
Elongation at Break 14 %14 %In 4D
 13 %
@Temperature -73.0 °C
13 %
@Temperature -99.4 °F
 13 %
@Temperature -184 °C
13 %
@Temperature -299 °F
 14 %
@Temperature 316 °C
14 %
@Temperature 601 °F
In 4D
 15 %
@Temperature 427 °C
15 %
@Temperature 801 °F
In 4D
 20 %
@Temperature 538 °C
20 %
@Temperature 1000 °F
In 4D
Reduction of Area 55 %55 %
 45 %
@Temperature -184 °C
45 %
@Temperature -299 °F
 50 %
@Temperature -73.0 °C
50 %
@Temperature -99.4 °F
 60 %
@Temperature 316 °C
60 %
@Temperature 601 °F
 65 %
@Temperature 427 °C
65 %
@Temperature 801 °F
 75 %
@Temperature 538 °C
75 %
@Temperature 1000 °F
Modulus of Elasticity 200 GPa29000 ksi
Notched Tensile Strength  1517 MPa
@Temperature -184 °C
220000 psi
@Temperature -299 °F
 2000 MPa
@Temperature 23.0 °C
290000 psi
@Temperature 73.4 °F
 2070 MPa
@Temperature -73.0 °C
300000 psi
@Temperature -99.4 °F
Poissons Ratio 0.300.30
Fatigue Strength 630 MPa
@# of Cycles 1.00e+7
91400 psi
@# of Cycles 1.00e+7
R.R. Moore Test, Smooth Rotating Beam
Shear Modulus 76.9 GPa11200 ksiCalculated
Charpy Impact 30.0 J22.1 ft-lbV-notch
 5.00 J
@Temperature -184 °C
3.69 ft-lb
@Temperature -299 °F
V-notch
 16.0 J
@Temperature -73.0 °C
11.8 ft-lb
@Temperature -99.4 °F
V-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000758 ohm-cm
@Temperature 23.0 °C
0.0000758 ohm-cm
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 22.0 - 93.0 °C
5.89 µin/in-°F
@Temperature 71.6 - 199 °F
 11.2 µm/m-°C
@Temperature 22.0 - 260 °C
6.22 µin/in-°F
@Temperature 71.6 - 500 °F
 12.0 µm/m-°C
@Temperature 22.0 - 482 °C
6.67 µin/in-°F
@Temperature 71.6 - 900 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 11 - 12.5 %11 - 12.5 %
Copper, Cu 1.5 - 2.5 %1.5 - 2.5 %
Iron, Fe 75 %75 %as remainder
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nb + Ta 0.10 - 0.50 %0.10 - 0.50 %
Nickel, Ni 7.5 - 9.5 %7.5 - 9.5 %
Niobium, Nb (Columbium, Cb) <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %
Tantalum, Ta <= 0.50 %<= 0.50 %
Titanium, Ti 0.80 - 1.4 %0.80 - 1.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)

NCAR7B / 15647

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.