MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® 58123 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.

Uses: Blown and flat die/cast film extrusion, injection molding and cable jacketing.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Water Vapor Transmission 420 g/m²/day27.0 g/100 in²/day50% RH; ASTM E96B
 3200 g/m²/day206 g/100 in²/day90% RH; ASTM D6701
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Time 5.00 sec
70
@Time 0.00139 hour
ASTM D2240
Tensile Strength 36.5 MPa5290 psiASTM D412
Elongation at Break 730 %730 %ASTM D412
100% Modulus 3.40 MPa
@Strain 100 %
493 psi
@Strain 100 %
ASTM D412
300% Modulus 5.50 MPa
@Strain 300 %
798 psi
@Strain 300 %
ASTM D412
Tear Strength 19.3 kN/m110 pliTrouser; ASTM D470
Graves Tear Strength 66.6 kN/m380 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 1717H18, 1000g; ASTM D3389
Tensile Set 6.0 %6.0 %200% elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °FDSC
Glass Transition Temp, Tg -70.0 °C-94.0 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 °C374 °FInjection
Middle Barrel Temperature 199 °C390 °FInjection
Front Barrel Temperature 215 °C419 °FInjection
Nozzle Temperature 215 °C419 °FInjection
Zone 1 171 °C340 °FExtrusion
Zone 2 177 °C351 °FExtrusion
Zone 3 182 °C360 °FExtrusion
Zone 4 188 °C370 °FExtrusion
Adapter Temperature 193 °C379 °F5, Extrusion
Die Temperature 193 °C379 °FZone 1, 6, Extrusion
 193 °C379 °FZone 2, Extrusion
Melt Temperature 150 °C302 °FKofler
 218 °C424 °FInjection
Mold Temperature 15.0 - 32.0 °C59.0 - 89.6 °FInjection
Drying Temperature 82.0 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Volume Swell in Water1.5%24hrs, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer

PNOVEON555 / 121446

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.