MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® 58123 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.

Uses: Blown and flat die/cast film extrusion, injection molding and cable jacketing.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Water Vapor Transmission 420 g/m²/day50% RH; ASTM E96B
 3200 g/m²/day90% RH; ASTM D6701
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 5.00 sec
ASTM D2240
Tensile Strength 36.5 MPaASTM D412
Elongation at Break 730 %ASTM D412
100% Modulus 0.00340 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00550 GPa
@Strain 300 %
ASTM D412
Tear Strength 110 pliTrouser; ASTM D470
Graves Tear Strength 380 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 17H18, 1000g; ASTM D3389
Tensile Set 6.0 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °CDSC
Glass Transition Temp, Tg -70.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 °CInjection
Middle Barrel Temperature 199 °CInjection
Front Barrel Temperature 215 °CInjection
Nozzle Temperature 215 °CInjection
Zone 1 171 °CExtrusion
Zone 2 177 °CExtrusion
Zone 3 182 °CExtrusion
Zone 4 188 °CExtrusion
Adapter Temperature 193 °C5, Extrusion
Die Temperature 193 °CZone 1, 6, Extrusion
 193 °CZone 2, Extrusion
Melt Temperature 150 °CKofler
 218 °CInjection
Mold Temperature 15.0 - 32.0 °CInjection
Drying Temperature 82.0 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
 
Descriptive Properties
Volume Swell in Water1.5%24hrs, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer

PNOVEON555 / 121446

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.