MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A897 Grade 5 (230-185-00 or 230-185-01) Austempered Ductile Iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: ASTM 897 (in-lb units) 230-185-00 or 230-185-01
ASTM 897M (SI units) 1600-1300-00.

Austempered Ductile Iron (ADI) offers low cost, design flexibility, good machinability, high strength-to-weight ratio and good toughness, wear resistance and fatigue strength because it can be cast like any other member of the Ductile Iron family, thus offering all the production advantages of a conventional Ductile Iron casting. Subsequently it is subjected to the austempering process to produce mechanical properties that are superior to conventional ductile iron, cast and forged aluminum and many cast and forged steels.

The mechanical properties of Ductile Iron and ADI are primarily determined by the metal matrix. The matrix in conventional Ductile Iron is a controlled mixture of pearlite and ferrite. (Tempered martensitic matrices may be developed for wear resistance, but lack the ductility of either as-cast Ductile Iron or ADI). The properties of ADI are due to its unique matrix of acicular ferrite and carbon stabilized austenite; called Ausferrite. ADI is a group of materials whose mechanical properties can be varied over a wide range by a suitable choice of heat treatment, as seen in the various entries in MatWeb.

The composition reported herein does not guarantee ADI properties, nor is it mandatory. However, this composition is a typical, industrially successful ADI composition. A good controlled chemistry like this one combined with a consistently high nodule count and nodularity and a consistent pearlite/ferrite ratio in clean, shrink-free Ductile Iron will provide the most robust process for the production of ADI.

Information supplied to MatWeb by Applied Process, Inc.

Key Words: ADI; ASTM A897M-15
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.0593 g/cc0.25503 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 460460B.I.D. 2.85 mm
Tensile Strength, Ultimate >= 1590 MPa>= 230000 psiMinimum
 1650 MPa240000 psiTypical
Tensile Strength, Yield >= 1280 MPa>= 185000 psiMinimum
 1450 MPa
@Strain 0.2 %
210000 psi
@Strain 0.2 %
Typical
Elongation at Break >= 1.0 %>= 1.0 %Minimum
 3.0 %3.0 %Typical; in 2 inch (50 mm) gage length
Reduction of Area 2.0 %2.0 %
Modulus of Elasticity 155 GPa22500 ksiStatic Young's Modulus
 163 GPa23700 ksiDynamic
Compressive Yield Strength 2520 MPa365000 psi
Poissons Ratio 0.250.25
Fracture Toughness 44.0 MPa-m½40.0 ksi-in½
Shear Modulus 62.1 GPa9010 ksi
Shear Strength 1480 MPa215000 psi
Charpy Impact 8.00 J
@Temperature 23.0 °C
5.90 ft-lb
@Temperature 73.4 °F
Charpy Impact, Unnotched 53.0 J
@Temperature 23.0 °C
39.1 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.5 µm/m-°C
@Temperature 20.0 °C
7.50 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 20.9 W/m-K145 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.7 %3.7 %
Copper, Cu <= 0.80 %<= 0.80 %
Iron, Fe 93 %93 %
Manganese, Mn 0.28 %0.28 %
Molybdenum, Mo 0.00 - 0.25 %0.00 - 0.25 %
Nickel, Ni <= 2.0 %<= 2.0 %
Silicon, Si 2.5 %2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A897/A897M-06 Grade 1 (130-90-09) Austempered Ductile Iron
ASTM A897 Grade 2 (150-100-07 or 150-110-7) Austempered Ductile Iron
ASTM A897 Grade 3 (175-125-04) Austempered Ductile Iron
ASTM A897 Grade 4 (200-155-01 or 200-155-02) Austempered Ductile Iron
SAE J2477 AD 1600 Automotive Austempered Ductile Iron

MDFEADI230 / 12070

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.