MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ASTM A897 Grade 3 (175-125-04) Austempered Ductile Iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: ASTM 897 (in-lb units) 175-125-04
ASTM 897M (SI units) 1200-850-04.

Austempered Ductile Iron (ADI) offers low cost, design flexibility, good machinability, high strength-to-weight ratio and good toughness, wear resistance and fatigue strength because it can be cast like any other member of the Ductile Iron family, thus offering all the production advantages of a conventional Ductile Iron casting. Subsequently it is subjected to the austempering process to produce mechanical properties that are superior to conventional ductile iron, cast and forged aluminum and many cast and forged steels.

The mechanical properties of Ductile Iron and ADI are primarily determined by the metal matrix. The matrix in conventional Ductile Iron is a controlled mixture of pearlite and ferrite. (Tempered martensitic matrices may be developed for wear resistance, but lack the ductility of either as-cast Ductile Iron or ADI). The properties of ADI are due to its unique matrix of acicular ferrite and carbon stabilized austenite; called Ausferrite. ADI is a group of materials whose mechanical properties can be varied over a wide range by a suitable choice of heat treatment, as seen in the various entries in MatWeb.

The composition reported herein does not guarantee ADI properties, nor is it mandatory. However, this composition is a typical, industrially successful ADI composition. A good controlled chemistry like this one combined with a consistently high nodule count and nodularity and a consistent pearlite/ferrite ratio in clean, shrink-free Ductile Iron will provide the most robust process for the production of ADI.

Information supplied to MatWeb by Applied Process, Inc.

Key Words: ADI; ASTM A897M-15
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.0779 g/cc0.25571 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 387387B.I.D. 3.10 mm
Tensile Strength, Ultimate >= 1210 MPa>= 175000 psiMinimum
 1310 MPa190000 psiTypical
Tensile Strength, Yield >= 862 MPa>= 125000 psiMinimum
 1100 MPa
@Strain 0.2 %
160000 psi
@Strain 0.2 %
Typical
Elongation at Break >= 4.0 %>= 4.0 %Minimum
 7.0 %7.0 %Typical; in 2 inch (50 mm) gage length
Reduction of Area 6.0 %6.0 %
Modulus of Elasticity 158 GPa22900 ksiStatic Young's Modulus
 167 GPa24200 ksiDynamic
Compressive Yield Strength 1930 MPa280000 psi
Poissons Ratio 0.250.25
Fatigue Strength  380 MPa
@# of Cycles 1.00e+7
55100 psi
@# of Cycles 1.00e+7
Reverse Bending, as machined
 415 MPa
@# of Cycles 1.00e+7
60200 psi
@# of Cycles 1.00e+7
rotating bending, as machined
Fracture Toughness 60.0 MPa-m½54.6 ksi-in½
Shear Modulus 63.2 GPa9170 ksi
Shear Strength 1170 MPa170000 psi
Charpy Impact 9.30 J
@Temperature 23.0 °C
6.86 ft-lb
@Temperature 73.4 °F
Charpy Impact, Unnotched 93.0 J
@Temperature 23.0 °C
68.6 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 21.5 W/m-K149 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.7 %3.7 %
Copper, Cu <= 0.80 %<= 0.80 %
Iron, Fe 93 %93 %
Manganese, Mn 0.28 %0.28 %
Molybdenum, Mo 0.00 - 0.25 %0.00 - 0.25 %
Nickel, Ni <= 2.0 %<= 2.0 %
Silicon, Si 2.5 %2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A897 Grade 2 (150-100-07 or 150-110-7) Austempered Ductile Iron
ASTM A897/A897M-06 Grade 1 (130-90-09) Austempered Ductile Iron
ASTM A897 Grade 5 (230-185-00 or 230-185-01) Austempered Ductile Iron
ASTM A897 Grade 4 (200-155-01 or 200-155-02) Austempered Ductile Iron
SAE J2477 AD 1600 Automotive Austempered Ductile Iron

MDFEADI175 / 12068

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.