MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Atom Adhesives AA-BOND 2112 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND 2112 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-sag characteristics. AA-BOND 2112 solvent-free adhesive is easily mixed and used for staking components to printed circuit boards for enhanced mechanical rigidity, and for bonding, laminating and repair applications involving metals, glass, ceramics, wood and many plastics. AA-BOND 2112 hardens to a tough, enamel-like coating offering good chemical resistance as well as superior physical and mechanical properties. The cured adhesive provides good electrical insulation and resistance to weather, galvanic action, petroleum products and lubricants, alcohol, salts, mild acids and alkalis, and other organic and inorganic compounds.

Appearance: Milky Translucent

Cure Type: Heat cure or Room Temperature

Benefits:

  • Tough enamel like cure
  • Bonds variety of substrates
  • Good electrical insulation
  • Weather resistant
Mix Ratio by weight: 100:22/Resin:Hardener

Substrates: metals, glass, ceramics, wood and many plastics

Typical Application: Printed circuit board repair, staking components, bonding, laminating and repair applications

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Solids Content 100 %100 %
Viscosity 60000 cP60000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Adhesive Bond Strength 13.1 MPa1900 psiAlum to Alum
Izod Impact, Notched 0.400 J/cm0.750 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+13 ohm-cm
@Temperature 100 °C
6.00e+13 ohm-cm
@Temperature 212 °F
Dielectric Constant 4.64.6
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°F
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 93.0 °C199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30.0 min30.0 min
 
Descriptive Properties
Thixotropic Index6.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PATOM008 / 172323

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.