MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

American Elements Tungsten Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Tungsten (W) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Tungsten Particles are typically 40-80 nanometers (nm) with specific surface area (SSA) in the 1 – 5 m 2 /g range. Nano Tungsten Particles are also available passivated and in Ultra high purity and high purity and coated and dispersed forms. Applications for Tungsten Nanocrystals include and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Coat tungsten particles with DNA and inject them into plant cells or plant embryos. Some genetic material will remain in the cells and transform them. This method allows transformation of plant plastids. The transformation efficiency is lower than in agro bacterial mediated transformation.

Key Words: Formula: W; CAS Number: 7440-33-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.040 - 0.080 µm0.040 - 0.080 µm
Specific Surface Area 1.0 - 5.0 m²/g1.0 - 5.0 m²/g
Molecular Weight 183.85 g/mol183.85 g/mol
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gold, Au
Overview of materials for 7000 Series Aluminum Alloy
Tantalum, Ta; Cold Worked
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 1000 Series Aluminum

EJAMER91 / 5574

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.