MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for 1000 Series Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "1000 Series Aluminum". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.70 - 2.71 g/cc0.0975 - 0.0979 lb/in³Average value: 2.70 g/cc Grade Count:72
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 12.0 - 55.012.0 - 55.0Average value: 32.1 Grade Count:29
Tensile Strength, Ultimate 45.0 - 205 MPa6530 - 29700 psiAverage value: 111 MPa Grade Count:35
Tensile Strength, Yield 10.0 - 165 MPa1450 - 24000 psiAverage value: 68.9 MPa Grade Count:34
Elongation at Break 1.00 - 50.0 %1.00 - 50.0 %Average value: 13.7 % Grade Count:34
Modulus of Elasticity 62.0 - 69.0 GPa8990 - 10000 ksiAverage value: 68.5 GPa Grade Count:35
Notched Tensile Strength 90.0 - 207 MPa13100 - 30000 psiAverage value: 145 MPa Grade Count:3
Ultimate Bearing Strength 117 - 241 MPa17000 - 35000 psiAverage value: 179 MPa Grade Count:4
Bearing Yield Strength 41.0 - 207 MPa5950 - 30000 psiAverage value: 116 MPa Grade Count:4
Poissons Ratio 0.3300.330Average value: 0.330 Grade Count:34
Fatigue Strength 20.7 - 62.1 MPa3000 - 9000 psiAverage value: 42.6 MPa Grade Count:11
Machinability 10.0 - 30.0 %10.0 - 30.0 %Average value: 20.0 % Grade Count:8
Shear Modulus 25.0 - 26.0 GPa3630 - 3770 ksiAverage value: 25.9 GPa Grade Count:34
Shear Strength 34.0 - 125 MPa4930 - 18100 psiAverage value: 73.4 MPa Grade Count:29
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000270 - 0.00000300 ohm-cm0.00000270 - 0.00000300 ohm-cmAverage value: 0.00000287 ohm-cm Grade Count:30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.8 - 25.5 µm/m-°C12.1 - 14.2 µin/in-°FAverage value: 24.0 µm/m-°C Grade Count:33
Specific Heat Capacity 0.900 - 0.904 J/g-°C0.215 - 0.216 BTU/lb-°FAverage value: 0.901 J/g-°C Grade Count:34
Thermal Conductivity 218 - 243 W/m-K1510 - 1690 BTU-in/hr-ft²-°FAverage value: 230 W/m-K Grade Count:31
Melting Point 643 - 660 °C1190 - 1220 °FAverage value: 652 °C Grade Count:29
Solidus 643 - 660 °C1190 - 1220 °FAverage value: 647 °C Grade Count:29
Liquidus 655 - 660 °C1210 - 1220 °FAverage value: 657 °C Grade Count:29
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.0400 - 0.05000.0400 - 0.0500Average value: 0.0467 Grade Count:9
Reflection Coefficient, Visible (0-1) 0.860 - 0.9600.860 - 0.960Average value: 0.889 Grade Count:11
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °FAverage value: 343 °C Grade Count:20
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 99.0 - 100 %99.0 - 100 %Average value: 99.5 % Grade Count:73
Beryllium, Be 0.000800 %0.000800 %Average value: 0.000800 % Grade Count:8
Boron, B 0.0100 - 0.0500 %0.0100 - 0.0500 %Average value: 0.0386 % Grade Count:14
Chromium, Cr 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0160 % Grade Count:15
Copper, Cu 0.00300 - 0.350 %0.00300 - 0.350 %Average value: 0.0561 % Grade Count:72
Gallium, Ga 0.00500 - 0.0300 %0.00500 - 0.0300 %Average value: 0.0268 % Grade Count:26
Iron, Fe 0.00600 - 0.800 %0.00600 - 0.800 %Average value: 0.284 % Grade Count:50
Magnesium, Mg 0.00600 - 0.300 %0.00600 - 0.300 %Average value: 0.0518 % Grade Count:51
Manganese, Mn 0.00200 - 0.300 %0.00200 - 0.300 %Average value: 0.0350 % Grade Count:68
Si+Fe 0.0200 - 1.00 %0.0200 - 1.00 %Average value: 0.683 % Grade Count:23
Silicon, Si 0.00600 - 0.350 %0.00600 - 0.350 %Average value: 0.158 % Grade Count:50
Titanium, Ti 0.00200 - 0.200 %0.00200 - 0.200 %Average value: 0.0312 % Grade Count:44
V+Ti 0.0100 - 0.0300 %0.0100 - 0.0300 %Average value: 0.0208 % Grade Count:13
Vanadium, V 0.00500 - 0.0500 %0.00500 - 0.0500 %Average value: 0.0469 % Grade Count:36
Zinc, Zn 0.00600 - 0.100 %0.00600 - 0.100 %Average value: 0.0572 % Grade Count:68

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 4000 Series Aluminum Alloy

M01040 / 81682

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.