VESTAMID® DX9302 BK E70178 has been developed for the production of flexible, impact resistant extruded parts, especially tubes. Its composition makes VESTAMID® DX9302 BK E70178 suitable for the extrusion of tubes for windshield washer systems that have only small amounts of extractables substances in water/alcohol mixtures. Further advantages of VESTAMID® DX9302 BK E70178 are the typical properties of PA 612 like little water adsorption, good dimensional stability and almost constant mechanical properties at changing ambient humidity. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Industrial Sector: Automotive and Mobility Processing: Extrusion Delivery form: Pellets, Granules Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels Electrical: Insulating Conformity: Automotive Additives: Unfilled Applications: Tube and hose Processing: Profile extrusion Special Characteristics: High impact strength, Light-stabilized, High heat resistant Color: Black Additives: Impact resistant, Conductive agent, Light stabilizer, Heat stabilizerInformation provided by Evonik. |