MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® DX9302 BK E70178 Nylon 612, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: VESTAMID® DX9302 BK E70178 has been developed for the production of flexible, impact resistant extruded parts, especially tubes. Its composition makes VESTAMID® DX9302 BK E70178 suitable for the extrusion of tubes for windshield washer systems that have only small amounts of extractables substances in water/alcohol mixtures. Further advantages of VESTAMID® DX9302 BK E70178 are the typical properties of PA 612 like little water adsorption, good dimensional stability and almost constant mechanical properties at changing ambient humidity. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion
Special Characteristics: High impact strength, Light-stabilized, High heat resistant
Color: Black
Additives: Impact resistant, Conductive agent, Light stabilizer, Heat stabilizer

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption 2.20 %2.20 %Sim to ISO 62
Moisture Absorption 0.500 %0.500 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.0190 cm/cm0.0190 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0120 cm/cm0.0120 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 33.0 MPa4790 psiISO 527
Tensile Strength 33.0 MPa4790 psiISO 527
Tensile Stress 31.0 MPa
@Strain 50.0 %
4500 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 31.0 MPa4500 psiISO 527
Elongation at Break >= 50.0 %>= 50.0 %Nominal; ISO 527
Elongation at Yield 15.0 %15.0 %ISO 527
Tensile Modulus 1.15 GPa167 ksiISO 527
Flexural Strength 38.0 MPa5510 psiISO 178
 46.0 MPa6670 psiat conv. Deflection; ISO 178
Flexural Modulus 1.17 GPa170 ksiISO 178
Flexural Strain at Break 7.00 %7.00 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.90 J/cm²
@Temperature -30.0 °C
9.04 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
Type of failure: P; ISO 179/1eA
Tensile Impact Strength 158 kJ/m²75.2 ft-lb/in²notched, atN, type of failure: C; ISO 8256/1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm?V; IEC 62631-3-1
Dielectric Constant  3.00
@Frequency 1.00e+6 Hz
3.00
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 3.80
@Frequency 100 Hz
3.80
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 41.0 kV/mm1040 kV/inAC, S20/P50; Sim to IEC 60243-1
 41.0 kV/mm1040 kV/inAC, S20/S20, t.; IEC 60243-1
Dissipation Factor  0.0310
@Frequency 1.00e+6 Hz
0.0310
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0470
@Frequency 100 Hz
0.0470
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 1.70 µm/m-°C
@Temperature 25.0 - 55.0 °C
0.944 µin/in-°F
@Temperature 77.0 - 131 °F
ISO 11359-1/-2
Melting Point 215 °C419 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Vicat Softening Point  110 °C
@Load 1.02 kg
230 °F
@Load 2.25 lb
50 K/h; ISO 306
 170 °C
@Load 5.10 kg
338 °F
@Load 11.2 lb
50 K/h; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °FInjection Molding; ISO 294
 260 °C500 °F
Mold Temperature 35.0 °C95.0 °FInjection Molding; ISO 294
 80.0 °C176 °F
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
 
Descriptive Properties
ColorBlack
Flexural stress at breakNMPa, ISO 178
 N%, ISO 178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7884 / 325016

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.