MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Pellethane® 5863-85A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Aromatic Polyether-based Thermoplastic Polyurethane (TPU)

Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.

Process: Extrusion and Injection Molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ASTM D2240
Tensile Strength, Ultimate 7000 psiASTM D412
Elongation at Break 570 %ASTM D412
100% Modulus 6.20 MPa
@Strain 100 %
ASTM D412
300% Modulus 10.3 MPa
@Strain 300 %
ASTM D412
Tear Strength 26.3 kN/mTrouser; ASTM D470
Graves Tear Strength 490 plidie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 37
@Load 1.00 kg
H-18; ASTM D3389
Tensile Set 14 %
@Temperature 200 °C
ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °C
 145 °CKofler
Glass Transition Temp, Tg -50.0 °C
 
Optical PropertiesOriginal ValueComments
Haze 1.8 %pressed between glass; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 177 °CInjection Molding
Front Barrel Temperature 182 °CInjection Molding
Nozzle Temperature 188 °CInjection Molding
Zone 1 171 °CExtrusion
Zone 2 177 °CExtrusion
Zone 3 182 °CExtrusion
Zone 4 188 °CExtrusion
Adapter Temperature 188 °CExtrusion, 5
Die Temperature 188 °CExtrusion
 188 °CExtrusion, 2
Melt Temperature 188 °CInjection Molding
Mold Temperature 15.0 °CInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® PC-3595A-B20 Aliphatic TPU
Lubrizol LifeSciences Pellethane® 2363-80A TPU
Lubrizol LifeSciences Pellethane® 2363-90AE TPU
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester

PLUBR9036 / 203603

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.